This case highlights how upgrading line shaft bushings and wear rings to GRAPHALLOY Nickel-grade materials helped a refinery overcome composite bushing failures caused by high-temperature, low-lubricity pentane service and solvent exposure. The result was a straightforward materials change that delivered years of reliable operation without altering pump geometry.